Swimming Pool Paint | 2K PU Paint

£79.99
  • Suitable to paint all pools (chlorine, saltwater, and mineral) indoors and outdoors
  • Properties: UV-resistant, elastic waterproof, highly durable, scratch resistant, and chemical resistant
  • Gloss Level: Available in matte or glossy
  • Consumption Volume: approx. 100g/m² per coat. We recommend approximately two coats.
  • Processing Temperature: +8°C to +35°C
  • Drying Time: Touch Dry/Walkable after 6h at 25°C
  • Scope of Delivery: Resin A-component, hardener B-component, and EP Colour Paste
Properties doubleChevron-black

1. Select colour

2. Select gloss level

Select gloss level
chevronBottom

3. Select quantity (m²) for 1 coat

Select quantity (m²) for 1 coat
chevronBottom

The Cost-Effective Alternative For Your Swimming Pool

EPODEX’s Swimming Pool Paint is not only more affordable than re-tiling or resurfacing — it also saves you from major renovation. Our 2K PU Paint can be applied in just a few simple steps. It helps prevent water infiltration and surface damage while giving your old pool a smooth finish with fewer micro-cavities. The result? A cleaner-looking pool that’s easier to maintain.

Instructions For Use

  1. Ensure the pool is sealed, stable, clean, dry, and free from any substances that may prevent proper adhesion. We recommend increasing the adhesion by sanding.
  2. Shake both components individually before use. Then, mix the resin A-component and the hardener B-component in a 3 to 1 mixing ratio (e.g. 1.5kg resin A-component with 0.5kg hardener B-component). Add 5% EP Colour Paste to the resin-hardener mixture to colour it (e.g. 100g EP Colour Paste to 2kg resin-hardener mixture).
  3. Stir through the edge and bottom of the mixing cup as the material will settle there. Ideally, pour into a clean mixing cup and mix again until the mixture is streak-free. This ensures that the resin A-component and hardener B-component are completely mixed together.
  4. Pour the mixture into a paint tray and apply it thinly with a roller in a criss-cross pattern.
  5. Let the first coat cure and apply the second coat in the same way. We recommend applying the second coat after min. 3h but not more than 20h.
  6. We recommend coating the walls before coating the bottom of the pool.
     

Pro Tip for Flooring:

Do not wear rubber-soled shoes while sanding, cleaning, after cleaning, or during the application of the 2K PU Paint, as rubber microparticles may cause an uneven finish. Rubber-soled shoes can be worn once the second coat of 2K PU Paint is cured. Wait until the 2K PU Paint is walkable (approx. 6 hours) before applying the second coat.

Professional-Grade Performance

Our Swimming Pool Paint is flexible, allowing it to tolerate thermal expansion and contraction — even through harsh winters! When applied properly, it won’t crack or peel come spring. Our 2K PU Paint is also UV resistant; unlike standard paints, it won’t yellow or degrade from sun exposure, leaving your pool looking as good as new for years to come. All these advantages are at your disposal for your next pool upgrade!

reviews

Danger 

Highly flammable liquid and vapour. May be fatal if swallowed and enters airways. May cause damage to organs through prolonged or repeated exposure. Causes skin irritation. May cause respiratory irritation. Flammable liquid and vapour. Harmful if inhaled. May cause an allergic skin reaction. May cause drowsiness or dizziness. Contains isocyanates. May produce an allergic reaction. The information on the product label must always be followed.